How to Mold This ‘Impossible’ Part
New low-pressure injection molding process “breaks the rules” and solves difficult molding problems.
First of all, it breaks a cardinal rule of injection molding: Flow from thick to thin, right? Well, this polypropylene part has a thick sprue that feeds two long, thin filaments, which feed into thick tunnel gates and relatively thick-wall, box-shaped parts (only one of which is shown here). Thick-to-(very) thin-to-thick again. Shouldn’t be done. Looks like it shouldn’t be possible.
And those filaments—talk about a flow-length to thickness (L/T) ratio! The filaments are 3 in. long × 0.030 in. diam. That’s a 100:1 L/T ratio.
So why do this at all? It’s a demonstration part handed out by iMFLUX, the six-year-old subsidiary of Procter & Gamble that developed a molding process that uses constant low pressure to overcome many of the drawbacks of conventional injection molding. The result is said to be higher part quality, with lower molded-in stresses, and faster cycles—not to mention savings from lower injection and clamp pressures.
This part demonstrates the degree of control engineered into the iMFLUX process to ensure constant low-pressure filling. Any hesitation in flow through those long, thin filaments would cause instant freeze-off.
Got you interested yet? Learn about the latest developments in this novel process and what molders, machine suppliers, and consultants are saying about it in a feature in the upcoming September issue, written by Gene Altonen, chief technology officer of iMFLUX. In the meantime, you can read an article he wrote for us last year, introducing the process.
Related Content
-
Back to Basics on Mold Venting (Part 1)
Here’s what you need to know to improve the quality of your parts and to protect your molds.
-
A Systematic Approach to Process Development
The path to a no-baby-sitting injection molding process is paved with data and can be found by following certain steps.
-
Got Streaks or Black Specs? Here’s How to Find and Fix Them
Determining the source of streaking or contamination in your molded parts is a critical step in perfecting your purging procedures ultimately saving you time and money.